In the present work, we undertake the preparation of chitosan nanofibers via electrospinning by varying solution concentration (1, 2, 3, 4 and 6 wt% (w/v)), applied voltage (14, 18 and 22 kV), flow rate (0.4 mL/h and 0.8 mL/h), needle diameter (0.2 mm and 0.8 mm) and distance between needle tip and collector (100 mm and 140 mm).