This study investigated the effect of nonrinse conditioners (ie, Ketac Nano Primer [KNP] and GC Self Conditioner [SC]) used as substrate pretreatment and their respective paste-paste resin-modified glass-ionomer cement (RMGIC) (ie, Ketac Nano [KN] and Fuji Filling LC [FF]) on microtensile bond strength to dentin and marginal sealing when compared with traditional RMGIC (ie, Photac Fil [PF] and Fuji II LC [FII]) used in association with polyacrylic acid (ie, Ketac Cavity Conditioner [KC] and GC Cavity Conditioner [CC]).